Group: Forum Members
Posts: 9,
Visits: 67
|
Hi all, just received the brand new TBC2 Through-Bag Connector, looks great thank you. However, I screwed the pieces together through a bit of resistance and now cannot unscrew (separate them). A few people had a go, with no luck. Stuck together solid. Any suggestions? When screwing them on, although there was a bit of resistance, I'm fairly sure I did not damage the thread.
|