Would it be possible to use you Carbon Skinning kit to cover a Mobility Scooter Body, Not sure what type of Plastic the scooter body is made of, I think it might be HDPE.
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi,

Very much depends exactly on the plastic type. Some inert plastics such as HDPE, Nylon etc are very hard to bond to so it may well delaminate from the original.  However it if is ABS or similar then a heavy key and roughening of the surface should be fine to get the resins to bond to. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search