CS25 SILICONE RUBBER
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ANTHONY DUNMORE
ANTHONY DUNMORE
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 5
HI GUYS,
I HAVE A PART I NEED TO CAST USING THE CS 25 SILICONE TO MOULD AROUND MY PART.
WHEN THE MOULD HAS BEEN CREATED AND THE ORIGINAL PART REMOVED I WOULD LIKE TO THEN TO US THE:
PX 30 FLEXIBLE RUBBER TO RE-CAST MY ORIGINAL..
DOES THE PX 30 RE-ACT WITH THE CS 25 SILICONE??
Reply
Like
3
Reply
Warren (Staff)
Warren (Staff)
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
The PX series of resins, being PU based will not stick to the silicone and should demould from the CS25 silicone no problem.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
CS25 SILICONE RUBBER
ANTHONY DUNMORE
-
6 Years Ago
The PX series of resins, being PU based will not stick to the silicone and should demould from the CS25 silicone no problem.
Warren (Staff)
-
6 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search