By ANTHONY DUNMORE - 4/25/2019 10:12:02 AM
HI GUYS, I HAVE A PART I NEED TO CAST USING THE CS 25 SILICONE TO MOULD AROUND MY PART.
WHEN THE MOULD HAS BEEN CREATED AND THE ORIGINAL PART REMOVED I WOULD LIKE TO THEN TO US THE: PX 30 FLEXIBLE RUBBER TO RE-CAST MY ORIGINAL..
DOES THE PX 30 RE-ACT WITH THE CS 25 SILICONE??
|
By Warren (Staff) - 4/25/2019 12:08:03 PM
The PX series of resins, being PU based will not stick to the silicone and should demould from the CS25 silicone no problem.
|
|