Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Carbon parts rippling/lumpy
Carbon parts rippling/lumpy
Post Reply
Like
3
Carbon parts rippling/lumpy
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
CmCarbon
C
CmCarbon
posted 6 Years Ago
ANSWER
HOT
Topic Details
C
Group: Forum Members
Posts: 19,
Visits: 239
Hi guys I'm having a issues. , my parts are perfect after being sanded and laquared but they keep going ripply and you can feel raised bits over it? Whys this happening? Iv been using xcr resin and also a poly resin.. both does the same thing.. I'm skinning parts.
Thanks
Reply
Like
3
Reply
MarkMK
MarkMK
posted 6 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 338,
Visits: 2K
Sounds like you're experiencing shrinkage of either the epoxy or polyester resin (not certain why you're using both in combination?)
This would happen more readily if the parts are exposed to heat above ambient temperatures after the initial cure, especially if exposed to strong sunlight. One way around this would be to post-cure at an elevated temperature following the initial coating stage, then do the final sanding to take away the uneven surface
Skinned parts generally are not so resilient to shrinkage, given the additional thickness of the resin coating, especially if exposed to natural light and heat etc.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Carbon parts rippling/lumpy
CmCarbon
-
6 Years Ago
Sounds like you're experiencing shrinkage of either the epoxy or polyester resin (not certain why you're using both in combination?) This would happen more readily if the parts are exposed to heat.....
MarkMK
-
6 Years Ago
I'm not using poly and epoxy together. Iv tryed both seperate and both do the same
CmCarbon
-
6 Years Ago
Again, it's most likely slight shrinkage of the resin following initial cure This will be more apparent if exposed to heat and a post-cure at elevated temperature is ideal. The parts will show signs...
MarkMK
-
6 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search