Hi!

i shaped a piece of foam into tube form and  wrapped it with unidirectional carbon fabric and cured it in room temperature. i did it this way cause foam is soft and  i wanted to make the tube stiff enough to wrap the next layers easily. now i want to place 6 layers of prepreg over this part. i will use shrink tape for consolidating next layers.
now my question is, can i wrap prepreg layers over this part? most probably i will cure the prepreg at 90 degree Celsius. since the base layer is made by hand layup process, i want to know if it can stand such temperature or it will deform under temperature. 

do i need to post cure the part first before wrapping it with prepreg? if yes in what temperature.

best regards,
hadi


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search