Group: Administrators
Posts: 167,
Visits: 4.6K
|
The GlassCast10, along with the '50,can cure with a few dimples/ripples in the open-to-air surface unlike GlassCast3 for example which will cure with a perfect, flat finish as a result of its superior self-leveling abilities. They will still be clear and glossy but may not be absolutely level.
|