Guys I want to know how much is the cycle of a wooden mold and one made out of steel. What i want to know is what's better for a mass production part. Let's say 1000 pieces. I believe steel will be less expensive, because we can use it to make more parts. What's your thought?
Replies
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
depends on what process you are using?? Prepreg / Infusion / Wet lay and what cure cycles you are using as temperature governs a lot of what the tool will be made from.
And also its geometry dependent as the mould will wear with use.


cvasilliou
c
Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)Supreme Being (128 reputation)
Group: Forum Members
Posts: 16, Visits: 102
scottracing - 4/2/2019 2:53:41 PM
depends on what process you are using?? Prepreg / Infusion / Wet lay and what cure cycles you are using as temperature governs a lot of what the tool will be made from.
And also its geometry dependent as the mould will wear with use.


lets say I am using prepreg process with a cure cycle on maximum 130 celcius. And we are talking for differently geometrys,where we make parts for a car(sidepod,nosecone,undertray,wings etc)