Hi Dennis,
It really does *have* to be chemical release agent. Easy-Lease works very well on glass and you'll probably find that you only need to apply it once to get maybe 20+ releases off glass. When you use the Easy-Lease, use a very small application cloth as mostly, it's the cloth, not the mould, that consumes the release agent.
All the best, Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|