Guys

I am after some advice please.

I've done a bit of wet layup and vacuum bag CF composite ( only simple stuff ! ) but am now looking to use infusion to create a flat panel ( approx 400mm x 900mm ) between two pieces of glass ( to be used as wing end plates on a hill climb car ). The construction would be :-

Gel coat-CF-Soric-CF-Gel coat

My question is, the two pieces of glass ( top and bottom mould ) will be larger than the composite stack so how do you stop the resin  taking the "easy route " around the composite stack and not wetting out the CF etc fully ? ( assuming the resin input is one end and the vacuum the other ).

Thanks in advance.

Adrian
Replies
Dennis G
Dennis G
Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)
Group: Forum Members
Posts: 34, Visits: 837
Just out of curiosity...When making a flat pannel do you draw the resin across the short side or the long side? Or os there a rule of thumb for all projects?

Thanks, Dennis
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)Composites Expert (Staff) (11K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Dennis,

Generall we would infuse across the shortest distance; there's no reason not to really and it just ensures that the infusion will run slightly faster. If it's impractical the infusing across the longer distance is OK but for obvious reasons it will take longer.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ARBMSPORT - 14 Years Ago
fgayford - 14 Years Ago
Matt (Staff) - 14 Years Ago
fgayford - 14 Years Ago
ARBMSPORT - 14 Years Ago
Matt (Staff) - 14 Years Ago
ARBMSPORT - 14 Years Ago
Dennis G - 14 Years Ago
Matt (Staff) - 14 Years Ago
Dennis G - 14 Years Ago
Matt (Staff) - 14 Years Ago
Dennis G - 14 Years Ago
Matt (Staff) - 13 Years Ago
Dennis G - 13 Years Ago
Matt (Staff) - 13 Years Ago
Dennis G - 13 Years Ago
Warren - 13 Years Ago
brasco - 13 Years Ago
Dennis G - 13 Years Ago
matthieutje65 - 13 Years Ago
Dennis G - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search