Hi Adrian,
Honestly, for motorsport use we almost never worry about UV protection. Parts we've been making for years (5 years at least) that have been used on occasional use track cars still look absolutely fine. Generally, they'll get smashed or be replaced/changed before UV damage would be a problem and even if they did start to discolour just slightly it's not the end of the world. On a road car that sits in the sun all day then it's a different story and unprotected parts could start to look quite shabby after just a year or two without some UV protection but for track use, most people would rather save a few grams (and the hassle) of paint.
--Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|