Guys

I am after some advice please.

I've done a bit of wet layup and vacuum bag CF composite ( only simple stuff ! ) but am now looking to use infusion to create a flat panel ( approx 400mm x 900mm ) between two pieces of glass ( to be used as wing end plates on a hill climb car ). The construction would be :-

Gel coat-CF-Soric-CF-Gel coat

My question is, the two pieces of glass ( top and bottom mould ) will be larger than the composite stack so how do you stop the resin  taking the "easy route " around the composite stack and not wetting out the CF etc fully ? ( assuming the resin input is one end and the vacuum the other ).

Thanks in advance.

Adrian
Replies
ARBMSPORT
ARBMSPORT
Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)
Group: Forum Members
Posts: 5, Visits: 367
Matt, Fred

Thanks very much for the replies.

Matt,  i have made some wet layup/vacuum cf panels on glass with no gel coat which have been ok. My concern is the UV protection aspect, bearing in mind the end use of the panel/sheet (motorsport) is UV protecting not really  necessary ? or should the sheet be clear coated ? ( i don't currently have any kit to spray two pack clear coat )

Thanks again.

Adrian
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Adrian,

Honestly, for motorsport use we almost never worry about UV protection. Parts we've been making for years (5 years at least) that have been used on occasional use track cars still look absolutely fine. Generally, they'll get smashed or be replaced/changed before UV damage would be a problem and even if they did start to discolour just slightly it's not the end of the world. On a road car that sits in the sun all day then it's a different story and unprotected parts could start to look quite shabby after just a year or two without some UV protection but for track use, most people would rather save a few grams (and the hassle) of paint.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ARBMSPORT - 13 Years Ago
fgayford - 13 Years Ago
Matt (Staff) - 13 Years Ago
fgayford - 13 Years Ago
ARBMSPORT - 13 Years Ago
Matt (Staff) - 13 Years Ago
ARBMSPORT - 13 Years Ago
Dennis G - 13 Years Ago
Matt (Staff) - 13 Years Ago
Dennis G - 13 Years Ago
Matt (Staff) - 13 Years Ago
Dennis G - 13 Years Ago
Matt (Staff) - 12 Years Ago
Dennis G - 12 Years Ago
Matt (Staff) - 12 Years Ago
Dennis G - 12 Years Ago
Warren - 12 Years Ago
brasco - 12 Years Ago
Dennis G - 12 Years Ago
matthieutje65 - 12 Years Ago
Dennis G - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search