Glasscast10/50 clear epoxy casting resin


Author
Message
S34n
S
Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)
Group: Forum Members
Posts: 18, Visits: 54
Can I use the 2:1 ratio method when dealing with small or large amounts of resin 
e.g.:-
16g resin would need 8g hardener
OR 
220g resin would need 110 hardener??
Thank you

Edited 6 Years Ago by S34n
Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Yes.