Hi,

Yes we would recommend GlassCast 3 for that kind of application. You may wish to brush a sealing coat over the tiles before doing the main pour of a couple mm thickness.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Ian Simmonds
I
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 1, Visits: 12
Can the clear floor resin be used with slate tiles to achieve an acrylic finish over the skate tiles?

Thanks

Ian
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search