By Ian Simmonds - 2/27/2019 6:53:33 PM
Can the clear floor resin be used with slate tiles to achieve an acrylic finish over the skate tiles?
Thanks
Ian
|
By Warren (Staff) - 2/28/2019 11:47:28 AM
Hi,
Yes we would recommend GlassCast 3 for that kind of application. You may wish to brush a sealing coat over the tiles before doing the main pour of a couple mm thickness.
|
|