Hi, How can I avoid bubbles in the castings when using Xencast (currently general purpose)? The mould is dry but there are always bubbles present, often on the surface ruining the castings.
Many Thanks
Reply
moeggesit
m
Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)Forum Member (47 reputation)
Group: Forum Members
Posts: 4, Visits: 9
Warren (Staff) - 2/12/2019 9:56:07 AM
I would say 15C or below is low.  Ideally 20C is the ballpark for most resins to perform at their best.

It is unusual for their to be a lot of bubbles in the P2 resin system , hence Rich asking if you had P6 as the P6 is more moisture and mixing sensitive.

The P2 is fairly forgiving as fast cast PU resins go, however it can still be effected by moisture and mixing issues.


Everything is done at an ambient of approx. 20C using dry plastic containers so there should not be any moisture. It's stirred to avoid ingress of bubbles. Would it help to warm it up before or during mixing/casting? Should the silicone moulds be heated to release moisture? How do you remove moisture? How do you mix without introducing bubbles. The bubbles form during curing process and is consistent throughout the final mould.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
moeggesit - 6 Years Ago
Warren (Staff) - 6 Years Ago
moeggesit - 6 Years Ago
Rich (Staff) - 6 Years Ago
moeggesit - 6 Years Ago
Warren (Staff) - 6 Years Ago
moeggesit - 6 Years Ago
Warren (Staff) - 6 Years Ago
Jimmyb - 5 Years Ago
Warren (Staff) - 5 Years Ago
Jimmyb - 5 Years Ago
Warren (Staff) - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search