Matting down epoxy resin


Author
Message
Charlie Davidson
Charlie Davidson
Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)
Group: Forum Members
Posts: 1, Visits: 1
I am filament winding a form with carbon fibre tow and epoxy resin. Any suggestions on how to matt down the glossy epoxy finish once it has set?

Hanaldo
Hanaldo
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Sand it with a suitably fine grit to match your desired look, or use a matte or satin clear coat.
Matthieu Libeert
Matthieu Libeert
Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hanaldo - 1/29/2019 8:19:31 AM
Sand it with a suitably fine grit to match your desired look, or use a matte or satin clear coat.

exactly what hanaldo is saying Smile 


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search