Talk Composites - The Forum for Advanced Composites

Matting down epoxy resin

http://www.talkcomposites.com/Topic31855.aspx

By Charlie Davidson - 1/29/2019 8:05:47 AM

I am filament winding a form with carbon fibre tow and epoxy resin. Any suggestions on how to matt down the glossy epoxy finish once it has set?
By matthieutje65 - 1/31/2019 4:11:49 PM

Hanaldo - 1/29/2019 8:19:31 AM
Sand it with a suitably fine grit to match your desired look, or use a matte or satin clear coat.

exactly what hanaldo is saying Smile