EPOXY NOT FLOWING ON WAX


Author
Message
ezsailor
ezsailor
Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)
Group: Forum Members
Posts: 20, Visits: 75
Just tried my first flat sheet 195g 2x2 c/f, and failed. I am using a polished aluminium table 2.4  x 1.7 Metres, No 8 wax, No 2 resin. I want a single thickness for decoration only. I waxed the Ali sheet and then tried to coat with epoxy, it kept producing pinholes which quickly opened up to bare circles the size of a penny. I brushed it over several times and gradually reduced the number of void circles but clouded the resin here and there, I assume with wax. I did press on and finish the sheet with Vac but had a persistent very slow leak, I just re pumped every 20 mins for 3 hours. The finished sheet (1/2mm thick) also shows tiny voids where the weave crosses. Perhaps I made some schoolboy errors here but a few hints would be much valued. I am wondering if everything was too cold at 12 deg?
Reply
ezsailor
ezsailor
Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)
Group: Forum Members
Posts: 20, Visits: 75
Mat.  Have taken the plunge and ordered the rest of the kit to infuse exactly as you advise. Will let you know how it goes.