Matt (Staff) (29/10/2012)
You're welcome!
Try infusing using the EL2 Laminating Resin. It will infuse slower than the IN2 infusion resin but it will still infuse (they're from the same family of resins). You will need to use a SLOW hardener (so if you purchase the FAST hardener then you'll want to pick up some of the AT30 SLOW to use with the resin instead) which will give the resin plenty of time to pull through before it gels.
--Matt
Hi Matt
I was talking to a epoxy manufacturer in LA about viscosity. He said that it would be Ok to add up to 8% acetone to the infusion resin to reduce the viscosity and reduce surface tention that can cause pin holes. I haven't tried it yet but will. I was wondering if you have ever heard of doing this or had experience with this technic?
Fred