Group: Forum Members
Posts: 4,
Visits: 25
|
Oh, both of your answers are very helpful. I am grateful for your input. I wasnt sure about using body filler, but I am very good at that type of thing. I wont be needing to produce hulls at an high rate. Perhaps 1 or 2 a week. I could easily use the body filler solution and keep the option to split the mold open if some problem arises.
|