I have some carbon parts with a few pinholes. How do I make them invisible in an easy way?
Regards
Frank
Edited 6 Years Ago by Frank
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Frank - 1/8/2019 12:05:15 PM
I have some carbon parts with a few pinholes. How do I make them invisible in an easy way?
Regards
Frank

Sand and recoat with epoxy or clearcoat a couple of times. You could also use CA glue to seal them or use a black filler if your ok with that 


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search