Talk Composites - The Forum for Advanced Composites

Cosmetic repair of pinholes

http://www.talkcomposites.com/Topic31556.aspx

By oberflaeche - 1/8/2019 12:05:15 PM

I have some carbon parts with a few pinholes. How do I make them invisible in an easy way?
Regards
Frank
By matthieutje65 - 1/8/2019 1:12:25 PM

Frank - 1/8/2019 12:05:15 PM
I have some carbon parts with a few pinholes. How do I make them invisible in an easy way?
Regards
Frank

Sand and recoat with epoxy or clearcoat a couple of times. You could also use CA glue to seal them or use a black filler if your ok with that