I am going to skin an existing panel and want to create the symmetrical matching effect down the middle.  As I am using dry carbon fibre how do you cut and align the edges to ensure you can get a perfect match. 

I was thinking of using some very light tack tape to hold the weave whilst I cut the carbon to size (Otherwise it just frays and you end up with loose strands).  Once I have applied the base coat and its got tacky, then lay on the carbon and pull off the tape.

Is there any other way this could be done ?


Reply
Lenny
Lenny
Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)Supreme Being (191 reputation)
Group: Forum Members
Posts: 16, Visits: 58
Thanks for all the replies guys.

As its only cosmetic, I think a little bit of hair spray will do the trick. (I'll pitch some off the missus when she's not looking).

I will check what carbon I have ordered previously, if i haven't got the profinish I might think of getting some.