EG 160 and air bubbles postcure


Author
Message
SHaas
S
Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)Supreme Being (387 reputation)
Group: Forum Members
Posts: 46, Visits: 383
Hi everybody,
I have the same problem with all EG160 moulds I prepared the last months: Taking the part out of the mould shows a perfect finish, but after postcuring in the recommended cycle there are points where it looks like air is trapped. But you could not see it before the curing process... any tips?

Regards and a wonderful christmas for everyone!

Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
You need to take more care with trapping air behind the surface coat - the air expands as it heats up, causing the blisters. 

Take your time to make absolutely sure there are no air bubbles behind the surface coat.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
SHaas - 7 Years Ago
Hanaldo - 7 Years Ago
cumberdale - 7 Years Ago
matthieutje65 - 7 Years Ago
SHaas - 7 Years Ago
matthieutje65 - 7 Years Ago
SHaas - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search