hi i want to make some pen blanks [ they will not be used for pens but are the same size ],they have to be made in 2 parts ,the centre being perspex rod,items placed on the perspex then resin over ,my question is then ,will the resin bond with the perspex ok ,i assume that i will use glasscast 10 for the resin
many thanks in advance
best regards  john
Reply
dewijohn
d
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Warren (Staff) - 11/14/2018 4:32:32 PM
GlassCast 10 will bond to perspex no problem. Be aware that using 2 different materials may result in a visible join from certain angles.

Hi Warren, many thanks for the answer. I'll do some clear ones first until I got the process right but will hopefully do the castings  over a darker base once sorted.again many thanks
Best regards john