By dewijohn - 11/14/2018 12:18:28 PM
hi i want to make some pen blanks [ they will not be used for pens but are the same size ],they have to be made in 2 parts ,the centre being perspex rod,items placed on the perspex then resin over ,my question is then ,will the resin bond with the perspex ok ,i assume that i will use glasscast 10 for the resin many thanks in advance best regards john
|
By dewijohn - 11/14/2018 4:54:27 PM
+xGlassCast 10 will bond to perspex no problem. Be aware that using 2 different materials may result in a visible join from certain angles. Hi Warren, many thanks for the answer. I'll do some clear ones first until I got the process right but will hopefully do the castings over a darker base once sorted.again many thanks Best regards john
|
|