Hi,

I want to utilize a cnc to make a mold from Foamular board or expanded polysterene.  I am looking for suggestions to coat the foam after machining so i can utilize the machined foam as a mold.  I have messed around a bit with the board and acetone melts the foam.
any suggestions?
Thanks,
Scott
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
spr11 - 10/3/2018 9:30:08 PM
Hi,

I want to utilize a cnc to make a mold from Foamular board or expanded polysterene.  I am looking for suggestions to coat the foam after machining so i can utilize the machined foam as a mold.  I have messed around a bit with the board and acetone melts the foam.
any suggestions?
Thanks,
Scott

One method is add a light layer of fibreglass cloth with epoxy resin over the foam surface first. The epoxy resin do not attack these foams.
Then you can add more coats of a suitable primer or resin to sand a better finish with and then you can mould from this. All depends on the details involved.

Another method is where you could add a thick coat of a tooling paste resin to the foam that can then also be CNC machined. You just need to CNC the original foam design a fraction smaller to allow for some paste thickness. Use epoxies or other that are safe with the foam.





Edited 8 Years Ago by Fasta
Warren (Staff)
Warren (Staff)
Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)Supreme Being (23K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Fasta is spot on with this one. The layer of fibreglass will give it a good degree of toughness making it harder to accidentally press through the thin layer of resin.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search