Companies that can CNC 2mm carbon fibre sheet from drawings


Author
Message
Sailing
S
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Forum Members
Posts: 4, Visits: 6
Having built some prototypes using your carbon fibre sheet, I need to get some parts CNC machined in 2mm single sided carbon fibre.  Can you recommend companies that can do this?

Reply
Sailing
S
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Forum Members
Posts: 4, Visits: 6
Steve Broad - 9/22/2018 2:55:26 PM
Sailing - 9/22/2018 12:24:59 PM
Having built some prototypes using your carbon fibre sheet, I need to get some parts CNC machined in 2mm single sided carbon fibre.  Can you recommend companies that can do this?

Any images of the parts? What sort of drawings?
Steve - and example drawing is below...