Hi, I'm planning on creating a worktop in the new kitchen, with biscuit cut sliced logs set in a clear resin with a layer perhaps 5-10mm above the wood  The wood will be approx 20mm thick, with resin in between and over . So overall thickness will be in the region of 30-40mm.Reading up I've worked out i'll need to seal the wood  But I'm stuck on working or how much resin I'll need. The overall area is 7 meters x 06 metres with a thickness of resin of 30mm, I'm thinking I can cut that in half at least because of the wood taking up the space so 15mm x 7m x .6m? Also would gc 50 be the ideal medium? Cheers
Reply
Danj
D
Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)Junior Member (23 reputation)
Group: Forum Members
Posts: 2, Visits: 5
Warren (Staff) - 9/14/2018 4:31:34 PM
For the large resin encapsulation projects similar to yours, GlassCast 50 Clear Epoxy Casting Resin is the ideal resin system to use.

The volume based on your measurements is 63 kg.



64kg? That seems a lot
Thanks, the big packs are on back order, I will talk to the boss and see what she thinks, £800 for a first go with resin is quite a gamble haha