Mould for air intake


Author
Message
Barnsley-Bill
B
Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)
Group: Forum Members
Posts: 25, Visits: 489
Hi all I want to make a split mould for this air intake for my car out of Pre peg ' I bought the uni mould kit but have since found out its no good with the higher temps with the pre peg
Could I use the glass fiber mesh out of the uni mould kit with the high temp resin and the EG60 Epoxy Tooling Gelcoat .

or if not can you make a split mould using the tooling pre peg ?


Hanaldo
Hanaldo
Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
No on both accounts unfortunately. The chopped strand mat that comes with the Unimould needs the styrene that is in the Unimould resins, it wont work with epoxy. And you can make a split mould with the tooling pre-preg, but not with the pattern you have. You need a solid pattern with rigid flanges, you cant have temporary barriers.

In all honesty, I would use the Unimould and hust use the low temp cure cycle. I've used the X-Preg system with vinylester tooling before and it works fine. Theres a few pinholes here and there, and if you need a service temperature higher than 80C then you need to do a post-cure out of the mould, but all of that is way less trouble than buying a whole new tooling system.
Barnsley-Bill
B
Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)
Group: Forum Members
Posts: 25, Visits: 489
Thanks
Hanaldo 
when you say 'if you need a service temperature higher than 80C then you need to do a post-cure out of the mould , is this once its cooked in the mould remove the part from the mould then put back in the oven by itsself on a higher temp  ?
Thanks.

Hanaldo
Hanaldo
Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
That's it. So follow the low temp cure cycle. When that has finished, demould the part, and put it back in the oven. If you have the precision control, it is best to do a very slow ramp rate of 0.1°C per minute up to your final cure temperature, then hold that temperature for an hour.
Steve Broad
Steve Broad
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 9/9/2018 9:42:20 AM
That's it. So follow the low temp cure cycle. When that has finished, demould the part, and put it back in the oven. If you have the precision control, it is best to do a very slow ramp rate of 0.1°C per minute up to your final cure temperature, then hold that temperature for an hour.

I would also bolt the two parts together prior to post curing, placing some release film between the flanges to remove any chance of them sticking together.

Hanaldo
Hanaldo
Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
What two parts? Surely this will be laid up as a single piece pipe?
Steve Broad
Steve Broad
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 9/9/2018 10:34:15 AM
What two parts? Surely this will be laid up as a single piece pipe?

I believe the plan is to make a split mould along the black line.

Hanaldo
Hanaldo
Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yes, but he isn't talking about the mould, he is talking about the final component. If he makes the mould using Unimould then his best bet when curing the pre-preg is to follow the low temp cure cycle followed by a free-standing post cure of the carbon fibre pipe to achieve maximum service temperature. 
Steve Broad
Steve Broad
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Hanaldo - 9/10/2018 12:06:49 AM
Yes, but he isn't talking about the mould, he is talking about the final component. If he makes the mould using Unimould then his best bet when curing the pre-preg is to follow the low temp cure cycle followed by a free-standing post cure of the carbon fibre pipe to achieve maximum service temperature. 

Yeah, being stupid again!

Barnsley-Bill
B
Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)Supreme Being (230 reputation)
Group: Forum Members
Posts: 25, Visits: 489

easy release the plug and mould 7 to 8 times and its stuck like super glue ? 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search