Hi everyone advise needed


Author
Message
Lee34
L
Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)
Group: Forum Members
Posts: 2, Visits: 34
Hello guys my name is lee. I'm a welder fabricator and composites is a hobby. I've made a few Fibreglass items with success thanks to the easy composites video tutorials. Anyway I'm looking to make some Fibreglass fairings for my motorbike for track use and want some advise for making the molds. Obviously I'll use the original fairings as the plug but How should I go about filling the openings where the headlights and tail lights go without modifying original fairing? I want to be able to reuse them. thanks in advance
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Lee34 - 9/4/2018 11:58:30 AM
Hello guys my name is lee. I'm a welder fabricator and composites is a hobby. I've made a few Fibreglass items with success thanks to the easy composites video tutorials. Anyway I'm looking to make some Fibreglass fairings for my motorbike for track use and want some advise for making the molds. Obviously I'll use the original fairings as the plug but How should I go about filling the openings where the headlights and tail lights go without modifying original fairing? I want to be able to reuse them. thanks in advance

You can temporarily fill small holes with Plasticine or wax, for bigger holes you can use a smooth material like the plastic core flute board and some hot glue to hold in place, then more wax to fill the remaining gaps.





Lee34
L
Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)
Group: Forum Members
Posts: 2, Visits: 34
Thanks for the reply problem is the openings are curved shapes so flat board won't work. Thought about leaving lights in and using wax to seal around them. Thoughts?
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
Lee34 - 9/4/2018 1:07:59 PM
Thanks for the reply problem is the openings are curved shapes so flat board won't work. Thought about leaving lights in and using wax to seal around them. Thoughts?

That will work and you could then add a vinyl image of the lights :-) You just need to make sure that you apply release agent properly otherwise you could damage the lights. That is the way I would do it, anyway :-)