How to make carbon plate with both faces finished


Author
Message
quinn
q
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 155, Visits: 992
Infusion seems to be the way to go, but you only get one finished face with peel ply texture on the other. What's the best way to get 2 finished faces? I tried a small 150mm square by just clamping 2 peices of aluminum tooling plate together and it worked perfect with really good fiber to resin ratio, but I need some larger 500x500 plates (2mm thick). I could use 2 plates of glass backed up by something else like mdf maybe, but I imagine just clamping around the outsides is not going to squeeze the middle well enough unless I get tricky with the clamping. Maybe some thick peices that span across with clamps on outside to hopefully put enough pressure in the middle. 
Any other good way to do this other than clamping? If clamping is the best option, what's the best choice of clamping plate material and method for doing it? 
Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
My limited experience tells me that 2mm thick panel made from any style of twill carbon will be bloody strong :-) The complete front clip of my car is mostly 2 layers of 220gm with 4 layers around the edges and a couple of stiffening ribs and weighs less than 7kg which includes the hinge mechanism and catches. With a twill there is no real need to orientate the weave although you could, if you wished, twist the 600gm layers 45 degrees.

I think 200gm is about 0.25mm thick so you would need 8 layers. Using a couple of 600gm layers sandwiched between 200gm cloth would do the job nicely and be a lot cheaper :-) Whether there are any issues with infusing thick carbon I will leave to the experts on here as I am a prepreg convert :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
scottracing - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
             +1
polaraligned - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
quinn - 7 Years Ago
                                 Gosh, yes, forgot about that :-)
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
quinn - 7 Years Ago
oekmont - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago
quinn - 7 Years Ago