+x Fasta - 8/17/2018 2:25:10 AMDid you also add some board flange areas to it?
+x Fasta - 8/13/2018 8:55:35 AM+x Warren (Staff) - 8/13/2018 8:24:51 AMHow does the fluff respond to a flap wheel? You could skim over it if it helps smooth the surface then coat with some Pattern-Coat PrimerI was thinking the same and have done this.Just impregnate the fluff with a primer and sand it smooth. Spray again if needed.
+x Warren (Staff) - 8/13/2018 8:24:51 AMHow does the fluff respond to a flap wheel? You could skim over it if it helps smooth the surface then coat with some Pattern-Coat Primer