Hello,
I recently bought the starter kit for VI. I follow the instructions in the video and I am getting a vacuum pressure of around -27.5 but when I clamp off the bag between the vacuum bag and the vacuum chamber, the vacuum gauge goes immediately up. Why is this happening? In the video it stays where it is. Is there a leak in the vacuum chamber? do you have any tips how to check this? many thanks