Hi all, I am new to Carbon Fibre, I have a Ferrari 458 which I would like to copy some parts in Carbon fibre, I have done quite a bit over the years with Glass Fibre, I even made a Mold of the complete Bodyshell of my Ferrari 308 GTS when I was restoring it + lots more smaller items, so now I would like to have a go at some Carbon Fibre bits, so any help appreciated I am based in co78se in Essex if anyone lives nearby you are always welcome to drop in anytime for a chat, Regards DM
Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
With your FG experience (making a complete body isn't a simple task) CF will be a breeze. It's like working with FG woven mat but with a much longer cure time.

I am in CM3 so not THAT far away :-)

Steve