Brand new to CF! Spark plug cover


Author
Message
LukeSGee
L
Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)
Group: Forum Members
Posts: 9, Visits: 44
Hi guys,

I’m currently trying to do research on producing a carbon fibre piece to replace my spark plug cover on my Honda. The piece looks like this..

https://www.heeltoeauto.com/images/P/oem_engine_dress_plugcvr_blk.jpg

The kit I have purchased to make the part is the following.

https://rover.ebay.com/rover/0/0/0?mpre=https%3A%2F%2Fwww.ebay.co.uk%2Fulk%2Fitm%2F162837289911

Am I able to just clean, apply release agent then coat the part in epoxy, allow to partly set tacky, lay fabric, wet out, lay second layer ect until thick enough then for the final layer allow to fully dry, apply epoxy coat layers up then wet sand, polish until glossy, finally just release the part from the Carbon piece?

I have just purchased a house so I’m on a unbelievably low budget unfortunately!

Thanks in advance!
Reply
LukeSGee
L
Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)
Group: Forum Members
Posts: 9, Visits: 44
Hi, cheers for your reply.

I’ve cancelled the order on the original kit I’ve bought. Considering ordering separately to hopefully save a bit of money..

Love the CRXs! Got any pictures?

I currently don’t have a mould to use, I was hoping to use the original part as a mould but it seems that it’s not possible.

I’m aware of how the basic process is carried out for mould making ect so I’ll have to buy some kit... what would be best to use, putty or fibreglass?

I’m just after making carbon fibre copies of engine/interior panels ect for aesthetics so I don’t really want invest a lot of money.

Also is vacuum bagging essential to making these cf panels or can it be avoided?

Again I appreciate the input. I’ve done a lot of research but coming up short!