GlassCast10 bubbles


Author
Message
amoss125
a
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 2, Visits: 7
Trying to use glasscast10 to fill a plastic honeycomb structure.
Mixing 2 to 1 ratio 100ml resin 50ml hardener with few drips of yellow pigment. After pouring over the plastic honeycomb and heating the resin it is nice and clear without any visible bubbles but during hardening over time i get small trailing bubbles building up. What am i doing wrong? do i need a pressure pot or do you think there is a reaction with the plastic honeycomb.

Reply
Nishitate Luis
N
Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)Forum Member (26 reputation)
Group: Forum Members
Posts: 4, Visits: 25
amoss125 - 6/25/2018 10:43:54 AM
Trying to use glasscast10 to fill a plastic honeycomb structure.
Mixing 2 to 1 ratio 100ml resin 50ml hardener with few drips of yellow pigment. After pouring over the plastic honeycomb and heating the resin it is nice and clear without any visible bubbles but during hardening over time i get small trailing bubbles building up. What am i doing wrong? do i need a pressure pot or do you think there is a reaction with the plastic honeycomb.