I am starting with creating a mold to recreate a side mirror outershel. Its not a cover but the real outershell. I like tot put the connection studs in the mold or glue them in after making the part.
Can you advise me how to achieve this? Is there a tutorial for the procedure?
Please let me know, so i can order some equipment. 


Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
There is not a set tutorial for that part but it is a relatively common moulding procedure.  You are likely to need a 2 part mould to make the part so you can easily release it from the mould.  You then have a couple of ways to make it, either resin infusion which could be a bit fiddly but is done at room temperature, or out of autoclave pre-preg would be easier to do, but needs an oven to cure.

I would have a look at our Online Composites Learning Area as we have videos covering the moulding process as well as both part making methods in detail.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search