Considering Making a Carbon Fiber Intake - Need guidance.


Author
Message
ihave2seats
i
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 5, Visits: 20
Hey, I'm new here but have always loved cars. This project will be for an Audi S4. For our car platform however, the intake options are less than ideal - otherwise I would buy one. 

An expensive but poor design:


This intake design is ideal, but it isn't for our car and serves as the inspiration for the project:


That said, my idea is to construct a snorkel that could work in conjunction with one of the heat shield only designs as such below:



Now, while I have never done any projects like this - I am pretty handy and learn quickly. I am looking to make a permanent mould, so that it can be replicated... but I have to design the shape first. I'm sure more questions will arise, but the two that I can think of are:
1. What is the best method to create an accurate mould?
2. If I make it a two piece that surrounds the filter, how do I set the threads for the screws to bolt down the lid? (See below for example):



Thank you SO MUCH in advance!!!
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It's sort of a bit grainy to tell, but they look like nutserts to me.

Heat resistance is all down to the resin you're using. If you're planning on wet laying these, there's quite a few high temperature resins that will handle 160+C with a post cure.  If you want to infuse you may struggle to find anything higher than 95-100, especially if you arent wanting to buy in bulk. Both wet lay and infusion will require a post cure up to the planned operating temperature in order to realise those temperature capabilities, so you would need a solution for getting them to that temperature for a few hours. Otherwise, if you have the facilities, pre-pregs will do about 120. 
ihave2seats
i
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 5, Visits: 20
Hanaldo - 6/19/2018 3:38:14 AM
It's sort of a bit grainy to tell, but they look like nutserts to me.

Heat resistance is all down to the resin you're using. If you're planning on wet laying these, there's quite a few high temperature resins that will handle 160+C with a post cure.  If you want to infuse you may struggle to find anything higher than 95-100, especially if you arent wanting to buy in bulk. Both wet lay and infusion will require a post cure up to the planned operating temperature in order to realise those temperature capabilities, so you would need a solution for getting them to that temperature for a few hours. Otherwise, if you have the facilities, pre-pregs will do about 120. 

Right, that makes sense. After looking a very hot IAT for this car would be around 87.50°C, so any of those would work. The pre-pregs 120 would be optimal. In addition to this, I would probably use a heat resistant clear coat. This leads me to another question - is there any way I could help reduce the internal temp of the intake by the construction of the CF? I read something about foamcore.

Sorry if this is a very simple question, but from the tutorial it looked like you could cure it in a regular oven as long as you ran the vacuum line outside to the pump. I only ask this because you mentioned having the facilities (in my mind that means special equipment! ha)

Based on your expertise, aside from the lid, would you see this being a two piece mould?

Edited 7 Years Ago by ihave2seats
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ihave2seats - 7 Years Ago
Hanaldo - 7 Years Ago
ihave2seats - 7 Years Ago
Hanaldo - 7 Years Ago
ihave2seats - 7 Years Ago
oekmont - 7 Years Ago
ihave2seats - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
ihave2seats - 7 Years Ago
Steve Broad - 7 Years Ago
Hanaldo - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search