https://store.acpsales.com/products/3485/the-cut-and-fold-technique
i saw that technique and i find it very intresting.but i dont fully understand this.when we fold the part to create an angle how is it possible the layer of carbon,that we dint cut with a dremel,to form that kind of angle without breaking?dont know if you understand what im trying to say.but if anyone is familiar with that technique maybe can help me or even send me some links to read and understand this better.  
thank you!
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The amount you can bend the panel depends on the thickness of the skin and its composition.  For example, a single layer of 200gsm twill carbon could be bent 180 degrees over a radius of around 100mm or even less. Smaller angles you might get a tighter radius of curvature.

If you knew where your bends are going to be, you could even engineer in a thinner laminate on a strip around the bend line . 


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search