I’m after your comments or suggestions. I’m having to make a mould to produce a carbon infused roof skin. This will bond to the outside margin of the original roof with the centre cut away.
My thoughts are, do I need to back off the edge Profile with sheet wax so the outside edge is slightly wider allowing the finished part to sit neatly over the original?
What have you guys experienced?
Thanks in advance.
Reply
flamypie
flamypie
Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)Supreme Being (80 reputation)
Group: Forum Members
Posts: 9, Visits: 45
Spot on. Thanks Warren.