Hello guys im planing to do seats by resin infusion can you advise what materials to you for a seats even of fiberglass best.

Thank you in advance guys

Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You will not find a concise list sadly.  The priority with such an item is crash safety, and that is what will determine what you use. Most typical composite materials can be made into race seats, including carbon, glass, aramid etc in a variety of weaves dependent on the design.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search