You would need to look closely at the original.  Tillet do glass and carbon composites, single and double skin etc so you need to have a good close look at what you are replicating. Obviously bear in mind you are copying a copyrighted design so you should really change your "pattern" sufficiently that it is no longer the same seat otherwise you could open yourself up to all sorts of litigation issues long before you get into  safety issues.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
Warren what can you suggest i made copy of Tillet B5 seat.

Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You will not find a concise list sadly.  The priority with such an item is crash safety, and that is what will determine what you use. Most typical composite materials can be made into race seats, including carbon, glass, aramid etc in a variety of weaves dependent on the design.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
Hello guys im planing to do seats by resin infusion can you advise what materials to you for a seats even of fiberglass best.

Thank you in advance guys

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search