guys this problem was nightmare to my friends parts also so errors caused him by these 2 spots : 1. VACUUMING BAD LEAKED! SECOND AND MAIN 2. MOLD YOU THINK YOU MADE GOOD BUT FROM PHOTO I SEE SAME ERROR ITS TINY HOLES IN YOUR MOLD THAT DO LEAKS FROM YOU AND PART NOT HAVE FULL VACUUMING AND YOU CAN NOT FIND ERROR. MY ADVISE DO NEW MOLD AS I THINK HERE YOU GETTING ERRORS.
|