Hello everyone,

I have a question regarding the bonding between a glass surface, and carbon fiber. I am building a table where the legs will be made of carbon fiber, and the top will be clear glass. I have seen glass being bonded to aluminum bases before with a clear epoxy (I am guessing its epoxy), but how would it be done with carbon fiber? Is there a clear adhesive that will attach the glass's slippery surface to the epoxy surface of the carbon fiber composite? Could I mix up some laminating epoxy (the same used for making the carbon fiber curves) and bond them together?

http://www.talkcomposites.com/Uploads/Images/e52a17f1-f553-46fa-b44c-5acf.png

This is a 3D model of the table I am trying to create. Hopefully it gives an idea of what I am talking about. Thanks in advance,

Mike
Dravis
Dravis
Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)Supreme Being (5.2K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
Epoxies bond very well to clean thoroughly degreased glass surfaces  (even to ones with inadequate release treatment, as I found out when trying to make my first piece of flat CF :blushSmile Silly me thought "Epoxy won't bond to glass ...."

An even better bond can be acheived if the bonding area can be lightly sandblasted (Mask off all the glass surface with heavy masking tape, except where you want the bonding surface.)  Normal "beadblasting media" will not work, this is glass beads.... You will need real Zirkon sandblasting media.

In some auto-parts shops you can buy a small "point area" sandblaster gun, they are usuallly cheap, and very usefull and comes with a small amount of blasting grit, for localised sandblasting of rust spots on cars, this will work fine.

Very nice, elegant design  Btw.  Smile

Good luck, and do post pics when ready to......

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
prairiecustomcomposites
prairiecustomcomposites
Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)Supreme Being (188 reputation)
Group: Forum Members
Posts: 26, Visits: 722
Thanks Dravis,

I believe you said in the introductory section that you were working on a chair and dining set. Do you have any pictures or a thread pertaining to it? I'd love to see some furniture work. I just think carbon fiber works really well for furniture from both a design and a structural point of view.

Mike
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search