amoss125
a
amoss125
posted 8 Years Ago
ANSWER
HOT
Topic Details
a
Group: Forum Members
Posts: 2,
Visits: 7
What pigments do you sell that are compatible with GlassCast 10
Reply
Like
5
Reply
Warren (Staff)
Warren (Staff)
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
The following solid colour pigments work well with GlassCast:
Epoxy Colour Pigment
For tints and translucent shades any of our tinting pigments would work:
Translucent Tinting Pigments
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
GlassCast 10 colours
amoss125
-
8 Years Ago
The following solid colour pigments work well with GlassCast: Epoxy Colour Pigment For tints and translucent shades any of our tinting pigments would work: Translucent Tinting Pigments
Warren (Staff)
-
8 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search