Hello.  I have a question.  Can I use stock car parts as the mold itself for creating carbon fiber parts? Some of the parts I want to currently make are:
Spark plug cover
Air box lid
Car emblem
Interior trim body pannels
Stock mud flaps
I currently have those parts but I'm not sure if I need to create a mold off of the original part and then create the carbon fiber part off of the mold, or If I can just use the original part as my mold.  I will be doing  the resin infusion method to create the carbon fiber parts.
Thank you in advance.
Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
oekmont - 4/26/2018 11:14:04 AM
An elan has very British tolerances anyways. The original bodywork had tolerances within an inch...

If it was made on a good day :-)

However, even cars built to closer tolerances can cope with carbon panels that are less than 1mm thick :-)

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Orlandodc2 - 7 Years Ago
Hanaldo - 7 Years Ago
oekmont - 7 Years Ago
Orlandodc2 - 7 Years Ago
Steve Broad - 7 Years Ago
Orlandodc2 - 7 Years Ago
oekmont - 7 Years Ago
Steve Broad - 7 Years Ago
oekmont - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search