Hi,

New to composites and would like some advice

I'm looking to achieve something similar to Adam Hansen's 'Hanseeno' cycling shoes - here's a video with him talking about them: https://cyclingtips.com/2014/05/adam-hansens-custom-shoes/

I've ordered a started kit and some unidirectional sheets from easycomposites and I've got a vague idea where to start.

I'm most worried about keeping the uppers flexible enough (Hansen talks about using a different resin there for this reason), and joining different parts to make a whole if I construct the shoes in sections.

Thanks
Luke
Reply
Mircea Andrei Ghinea
M
Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)Forum Member (31 reputation)
Group: Forum Members
Posts: 5, Visits: 346
ljac133 - 4/20/2018 12:47:46 PM
Hi,

New to composites and would like some advice

I'm looking to achieve something similar to Adam Hansen's 'Hanseeno' cycling shoes - here's a video with him talking about them: https://cyclingtips.com/2014/05/adam-hansens-custom-shoes/

I've ordered a started kit and some unidirectional sheets from easycomposites and I've got a vague idea where to start.

I'm most worried about keeping the uppers flexible enough (Hansen talks about using a different resin there for this reason), and joining different parts to make a whole if I construct the shoes in sections.

Thanks
Luke

Hi, Luke! 
Did you manage to work with the EF80 flexible resin?
Interestingly :-) i am thinking to try doing the same thing as you here.
Best regards,
Mircea 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
ljac133 - 7 Years Ago
Warren (Staff) - 7 Years Ago
Mircea Andrei Ghinea - 6 Years Ago
ljac133 - 6 Years Ago
Mircea Andrei Ghinea - 6 Years Ago
ljac133 - 6 Years Ago
Mircea Andrei Ghinea - 6 Years Ago
ljac133 - 6 Years Ago
Mircea Andrei Ghinea - 6 Years Ago
mathboy - 6 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search