Hello guys I am new here. Congrats to all of you for the great work.I am using carbon fiber pre-preg that cures for 2 hours at 175 degrees . Is it possible to cure at 50 degrees for much more time ?
Reply
Kanou
Kanou
Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)Junior Member (19 reputation)
Group: Forum Members
Posts: 2, Visits: 71
Thanks guys for all the support. I will take into consideration all the above & I will notify you for the results of my experiment.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search